    Hello Friends,

    Will it be possible for someone to let me know on various methods that can be applied for OD Corrosion (Pitting type) where UT Readings cannot be carried out. Also which is the best method that we should go for??

    #4306
    Zayne Albutt
    Zayne Albutt
    Participant

    Hi,

    Have you considered using 3D Scanning using structured light. We are agents and service providers for Seikowave.

    You will be able to get more info from their website.

    https://energy.seikowave.com/energy-seikowave-com

    #4722
    Surya
    Surya
    Participant

    Laser based techniques also becoming popular to image the pitting on the external surface. Both 3D structured light technique and Laser based techniques are emerging in innovation and software options that enable the user to calculate the burst pressure calculations with the reduced thickness quickly and effectively so end user can set the pressure limits or take a call on repair based on the results. Seikowave I have personally used and its a good tool to image the corrosion/ pitting on the external surface. However, to be successful in using this light based techniques over exposure of the test surface (due to sunlight) has to be eliminated.

    #7232

    Have you considered using 3D Scanning using structured light. We are agents and service providers for Seikowave.